Waterproofing on a Wall
Repair and waterproofing stucco wall in ready-mixed and mixed polymers to improve mixing in the field.
All existing concrete surfaces must be cleaned with tap water and to make sure no water leaks. Places to leak should be marked before contacting Technical room for advice or support. Use water quality Sika 102 and Sikagrout 212-11 where water leaks prior to mortar Sika Latex.
I. MATERIALS
Sika Latex Mortar improvement Flatten preliminary rough concrete surface.
107 Sikatop Seal grout waterproof polymer and silicafume improvement.
Sikagrout 212-11 Block leaking if required.
Sika 102 Block leaking water if required.
II. CONDITIONS CONCRETE
Construction quality connections at work and mortar Sika Latex (under the guidance of The Advanced Technology Sika Latex) to the concrete surface to surface roughness suitable for construction and waterproofing coating.
III. WATERPROOFING COATINGS
• Construction of two class Sikatop Seal 107 (density of about 1.5 kg/m2/lop) with viscosity as mortar to the concrete surface was saturated with natural bristle brush or sprayer and wet plaster to dry product 4 - 8 hours. Airport construction in the second layer to achieve perfect flat surface.
All existing concrete surfaces must be cleaned with tap water and to make sure no water leaks. Places to leak should be marked before contacting Technical room for advice or support. Use water quality Sika 102 and Sikagrout 212-11 where water leaks prior to mortar Sika Latex.
I. MATERIALS
Sika Latex Mortar improvement Flatten preliminary rough concrete surface.
107 Sikatop Seal grout waterproof polymer and silicafume improvement.
Sikagrout 212-11 Block leaking if required.
Sika 102 Block leaking water if required.
II. CONDITIONS CONCRETE
Construction quality connections at work and mortar Sika Latex (under the guidance of The Advanced Technology Sika Latex) to the concrete surface to surface roughness suitable for construction and waterproofing coating.
III. WATERPROOFING COATINGS
• Construction of two class Sikatop Seal 107 (density of about 1.5 kg/m2/lop) with viscosity as mortar to the concrete surface was saturated with natural bristle brush or sprayer and wet plaster to dry product 4 - 8 hours. Airport construction in the second layer to achieve perfect flat surface.

Other
- Waterproofing on a Wall( 12-08-2011 )
Vietthai trading co.,ltd Head Office: Lot. K81C Thu Trung - Dang Lam – Hai An Dist – Hai Phong City, VietnamTel: 0313.558.619 / Fax: 0313.558.690 Email: chivietthai@chongtham.vn Website: www.Chongtham.vn :: www.vietthaico.com |
Branch in Hanoi P202 - C6 Building Blocks 2 - My Dinh 1 Urban - Tran Huu Duc St - Tu Liem Dist – Ha Noi City, VietnamTel: +84-4-6287 4144 / Fax: +84-4-6287 4147 Email: vietthai@chongtham.vn Website: www.Chongtham.vn :: www.vietthaico.com |